200 ton SS 304 2 B Plate S275JR Low Carbon Steel Checkered Plate skickas till Sydkorea
Jul 10, 2025
Lämna ett meddelande
In this order, the customer requested to check carefully the material SS304 is 2B surface with 2.5mm, 3mm, 4mm and 5mm. And the width is 1m, 1.2m and 2.4m with the length is 9.5m.And the Mild Steel Chequered Plate is 3mm with special size with 1.55mx 3.1mm or 2.35mx 2.35m



|
Materiell förfrågan |
191,296.33 |
||||||||
|
Sn |
Material |
Thk |
Densitet |
Bredd |
Längd |
Vikt |
Antal |
T . vikt |
Enhet |
|
1 |
SS 304 2 B |
2.5 |
8 |
1.2 |
8.4 |
201.60 |
1 |
201.60 |
kg |
|
2 |
SS 304 2 B |
2.5 |
8 |
1.8 |
6.4 |
230.40 |
2 |
460.80 |
kg |
|
3 |
SS 304 2 B |
2.5 |
8 |
2 |
9.5 |
380.00 |
48 |
18,240.00 |
kg |
|
4 |
SS 304 2 B |
3 |
8 |
1 |
9.5 |
228.00 |
48 |
10,944.00 |
kg |
|
5 |
SS 304 2 B |
3 |
8 |
1.2 |
8 |
230.40 |
3 |
691.20 |
kg |
|
6 |
SS 304 2 B |
3 |
8 |
1.2 |
9.5 |
273.60 |
3 |
820.80 |
kg |
|
7 |
SS 304 2 B |
3 |
8 |
1.219 |
6.096 |
178.34 |
2 |
356.69 |
kg |
|
8 |
SS 304 2 B |
3 |
8 |
1.524 |
6.096 |
222.97 |
9 |
2,006.71 |
kg |
|
9 |
SS 304 2 B |
3 |
8 |
2 |
9.5 |
456.00 |
20 |
9,120.00 |
kg |
|
10 |
SS 304 2 B |
3 |
8 |
2.4 |
9.5 |
547.20 |
20 |
10,944.00 |
kg |
|
11 |
SS 304 2 B |
4 |
8 |
1.524 |
6.096 |
297.29 |
14 |
4,162.06 |
kg |
|
12 |
SS 304 2 B |
4 |
8 |
2.4 |
9.5 |
729.60 |
20 |
14,592.00 |
kg |
|
13 |
SS 304 2 B |
5 |
8 |
1.2 |
9.5 |
456.00 |
24 |
10,944.00 |
kg |
|
14 |
SS 304 2 B |
5 |
8 |
1.524 |
6.096 |
371.61 |
31 |
11,519.98 |
kg |
|
15 |
S275JR |
16 |
7.85 |
1.524 |
6.096 |
1,166.86 |
10 |
11,668.62 |
kg |
|
16 |
S275JR |
20 |
7.85 |
1.524 |
6.096 |
1,458.58 |
10 |
14,585.78 |
kg |
|
17 |
S275JR |
25 |
7.85 |
1.524 |
6.096 |
1,823.22 |
10 |
18,232.22 |
kg |
|
18 |
Rutig 3mm |
3 |
7.85 |
1.55 |
3.1 |
113.16 |
100 |
11,315.78 |
kg |
|
19 |
Rutig 3mm |
3 |
7.85 |
2.35 |
2.35 |
130.05 |
18 |
2,340.99 |
kg |
|
20 |
S275JR |
12 |
7.85 |
1 |
9.5 |
894.90 |
20 |
17,898.00 |
kg |
|
21 |
S275JR |
12 |
7.85 |
1.2 |
6.5 |
734.76 |
9 |
6,612.84 |
kg |
|
22 |
S275JR |
12 |
7.85 |
1.524 |
9.5 |
1,363.83 |
10 |
13,638.28 |
kg |
Skicka förfrågan