As one of the top ten stainless steel exporters in China, GNEE focuses on customized production of {{0}}grade stainless steel coils (UNS S20100, GB\/T 20878 12Cr17Mn6Ni5N), with an annual export volume of 100,000 tons, and products covering 50+ countries around the världen (som Sydostasien, Mellanöstern och Latinamerika). Relying on the full-process automated production line (Germany's SMS cold rolling mill, Japan's Koyo slitting line), we can achieve full-specification customization from 0.2mm ultra-thin strips to 15mm hot-rolled coils, strictly following international standards such as ASTM A240, JIS G4305, and EN 10088, and provide cost-effective material solutions for industries such as building decoration, home appliance manufacturing, och hårdvarubehandling.

 

 

Anpassningsbara stålspolarspecifikationer 201

Punkt Konventionell sortiment Anpassningsförmåga Exportstandarder
Materiell 201 (12cr17mn6ni5n) 201CU (kopparinnehållande typ, stämpelprestanda +15%) GB\/T 20878, ASTM A276, JIS G4303
Tjocklek Kallrullad: 0. 2-3. 0 mm
Hot-rolled: 1. 5-15 mm
Ultra-tunn 0. 15mm (Precision Strip), extra tjock 20mm Tjocklek tolerans: kallrullad ± 0. 0 3mm, varmvalsad ± 0,1 mm
Bredd Kallrullad: 50-1250 mm
Hot-rolled: 600-1500 mm
Smal remsa {{0}} mm (Slitting Precision ± 0,01mm) Breddtolerans: ± {{0}}. 5mm (standard)\/±0,1mm (precision)
Ytfin 2B (kallrullad matt), BA (ljus glödgad), HL (borstad) 8k spegel (glans större än eller lika med 85GU), PVD -titanplätering (färgad) ISO 10110 Optisk inspektion, ytråhet RA mindre än eller lika med 1,6μm
Hårdhetsvillkor 1\/4H (hv 180-220), 1\/2h (hv 250-300) Fullhårt tillstånd (hv 500+, lämplig för vårremsor) JIS HRC -hårdhetstest, fel ± 5HV

 